Cast Aluminum Alloys
|
|
Alloy
|
Tensile
PSI
|
Yield
PSI
|
Elong.
%
|
Brinnell
|
|
ALLOY A356:
|
27,000
|
13,000
|
8.0%
|
75
|
|
-high tensile strength
|
|
|
|
|
|
-machinability
|
|
|
|
|
|
|
|
|
|
|
|
ALMAG 35(535):
|
38,000
|
20,000
|
9.0%
|
70
|
|
-high tensile strength
|
|
|
|
|
|
-machinability
|
|
|
|
|
|
|
|
|
|
|
|
TENZALLOY (713)*:
|
36,000
|
26,000
|
5.0%
|
74
|
|
-high strength
|
|
|
|
|
|
|
|
|
|
|
|
ALLOY 319:
|
27,000
|
18,000
|
2.0%
|
70
|
|
-general low cost uses
|
|
|
|
|
|
|
|
|
|
|
|
ALLOY 355*:
|
27,500
|
15,500
|
3.5%
|
75
|
|
-pressure tight applications
|
|
|
|
|
|
|
|
|
|
|
|
ALLOY A357
|
54,000
|
45,000
|
3.0%
|
95
|
|
-high fatique properties
|
|
|
|
|
|
-impact properties
|
|
|
|
|
|
|
|
|
|
|
|
|
*- heat treatable for increased
mechanical properties
|
|